The requirement of High Solids Content, Cold Liquid-Applied Elastomeric Waterproofing Membrane Physical Requirements as per ASTM C 836 - 00 / 03 are as follows:
Testing specimen shall be as follows:
Pull it in a direction normal to the break, at a separation rate of 12.7 mm (0.5 in.)/min, until the distance between the bench marks is exactly 57.2 mm (2.25 in.). Stop the machine and immediately examine the films for any breaks or cracks. There shall not be any cracking or tearing of the film along the opened area on any of the three specimens.
Detail testing procedure is available in ASTM C 1305 and 1305M.
Testing specimen shall be as follows:
Pull it in a direction normal to the break, at a separation rate of 12.7 mm (0.5 in.)/min, until the distance between the bench marks is exactly 57.2 mm (2.25 in.). Stop the machine and immediately examine the films for any breaks or cracks. There shall not be any cracking or tearing of the film along the opened area on any of the three specimens.
Detail testing procedure is available in ASTM C 1305 and 1305M.
Many thanks to google.com and doc88.com from where the details have been collected.